How hard is your metal?

Enter the test load, the ball diameter and the diameter of the dent: get the Brinell hardness number, the depth, the validity check and the estimated tensile strength.

Updated on
Your inputs

Value out of range

Value out of range

Value out of range

Results

Brinell hardness (HBW)

228.8

Indentation ratio d ÷ D
0.400
Valid test: the indentation is between 0.24 D and 0.6 D
Depth of the indentation
0.417 mm
Load factor F ÷ D²
30.0 kgf/mm²
Estimated tensile strength of steel
789 MPa

The Brinell hardness test presses a hard steel or carbide ball into a metal surface under a known load, then measures the diameter of the dent. A softer metal gives a wider dent, a harder one a smaller dent. This calculator turns the load, the ball diameter and the indentation diameter into the Brinell hardness number (HBW), and checks that the test meets the standard conditions.

How the calculation works

  • Hardness HB = 2F ÷ (π × D × (D − √(D² − d²))), with F in kgf and the diameters in mm
  • Depth of the indentation = (D − √(D² − d²)) ÷ 2
  • Indentation ratio = d ÷ D, which should lie between 0.24 and 0.6
  • Load factor = F ÷ D²
  • Tensile strength of steel ≈ 3.45 × HB, in MPa

Example

A steel part is tested with a 10 mm ball under a load of 3,000 kgf, and the dent measures 4.0 mm. The depth is 0.417 mm, and the hardness is 228.8 HBW. The ratio d ÷ D is 0.4, inside the valid range, and the load factor is 30, the usual value for steel. The estimated tensile strength is about 789 MPa.

Where it is used

Brinell testing suits castings, forgings and other coarse-grained metals, because the large dent averages over the structure. It is used for quality control of steel, cast iron and aluminium, and for checking heat treatment. Because the dent is big, it is not suited to thin parts, small parts or hardened surfaces, where a Rockwell or Vickers test is a better choice.

Good to know

Measure the dent in two perpendicular directions and use the average. Test on a flat, clean surface, at least 2.5 times the dent diameter from an edge. The sample thickness should be at least ten times the depth of the dent. A Brinell number has no unit, although it is in kgf per mm² by definition, and converting to other hardness scales is only approximate.

For the stiffness and stress of a part, use the Hooke’s law calculator or the beam deflection calculator. The strain gauge calculator turns small deformations into stress readings.

Frequently asked questions

What does HBW 10/3000 mean?

A Brinell test with a tungsten carbide ball of 10 mm and a load of 3,000 kgf. The hardness number is usually written first, such as 229 HBW 10/3000.

What load should I choose?

Use a load factor F ÷ D² of 30 for steel and cast iron, 10 for copper alloys and 5 for aluminium and softer metals, so that the dent stays in the valid size range.

Can I estimate the tensile strength from hardness?

For carbon and low-alloy steels, the ultimate tensile strength in MPa is about 3.45 times the Brinell hardness. It is a rough guide, not a substitute for a tensile test.

Why must the indentation be between 0.24 D and 0.6 D?

Smaller dents are hard to measure accurately, and larger ones are affected by the shape of the ball and the thickness of the sample. Outside the range the standard does not accept the result.