Skip to content
Omnikalc

Galvanized coating zinc mass and service life calculator

Enter the zinc coating thickness, the environment and the surface of the steel to get the zinc mass per area, the total zinc, the zinc left after 25 years and the time to first maintenance.

Updated on
Your inputs
mils

Value out of range

ft²

Value out of range

Results

Time to first maintenance

52.8 years

Zinc coating mass
2.32 oz/ft²
Zinc on the whole surface
724 lb
Zinc left after 25 years
61.6 µm

The galvanized coating calculator gives the zinc mass per area, the total zinc on a surface of steel, the zinc left after 25 years and the time to first maintenance of a hot-dip galvanized coating, from its thickness, the corrosion environment and the surface of the steel.

How the calculation works

  • Enter the thickness of the zinc coating in mils.
  • Choose the environment, which sets the corrosion rate of the zinc.
  • Enter the surface of the steel to get the coating mass, the zinc on the surface, the zinc left after 25 years and the time to first maintenance.

Example

A hot-dip galvanized coating of 3.9 mils is 3.9 × 25.4 = 99.1 µm thick. Its mass is 99.1 × 7.14 = 707 g/m², that is 2.32 oz/ft². For 5,000 ft² of steel, the zinc weighs 724 lb. In a suburban environment at 1.5 µm/year, 61.6 µm are left after 25 years, and the first maintenance comes after 99.1 × 0.8 / 1.5 = 52.8 years.

Why it matters

The calculator helps engineers, architects, fabricators, galvanizers and owners to compare the life of a galvanized steel in different environments, to estimate the zinc used on a structure, and to plan the maintenance of a bridge, a fence, a tower or a guardrail.

Good to know

Use the coating thickness measured on the real parts and not only the minimum of the standard. Choose a thicker coating or a duplex system with paint for the marine and industrial environments. Avoid the contact of the zinc with copper and with wet concrete that is not cured, and inspect the coating every few years, because a local repair with zinc-rich paint is easy while the damage is small.

The corrosion rate calculator converts a mass loss into a rate, the thermal expansion calculator gives the change of length of a steel member, the spray applied fireproofing thickness calculator gives the fireproofing of steel and the steel column capacity calculator checks a steel column.

Frequently asked questions

How is the zinc mass found?

The mass of the coating per unit of area is the thickness times the density of zinc, which is 7.14 g/cm³. A coating of 100 µm weighs about 714 g/m². In American units, 1 oz/ft² of zinc is 305 g/m², or a thickness of about 1.7 mils. The total zinc is the mass per area times the surface of the steel.

How long does a galvanized coating last?

The zinc corrodes slowly and protects the steel even where the coating is scratched. The life is the thickness divided by the corrosion rate of the environment, which is about 0.7 µm/year in the country and 5 µm/year in a severe marine or industrial setting. The calculator gives the time to the point where 80 % of the zinc is gone, when the first maintenance is advised.

What thickness should I expect?

The standard for hot-dip galvanizing of fabricated steel gives a minimum average coating from about 1.4 to 3.9 mils, according to the thickness of the steel and the category of the item. Thicker steel receives a thicker coating. Check the product standard and the mill report for the real value, and measure it with a magnetic gauge.

What are the limits of the calculator?

The calculator uses constant corrosion rates and does not include the local conditions, such as the splash zone, the deicing salts, the wet and dry cycles, the contact with other metals or the pollution. It does not apply to the duplex coating, where paint is added over the zinc. Use the corrosion map of your region and the data of the galvanizer.

Was this calculator helpful?

Thanks for your feedback!

Results are estimates provided for information purposes. They do not replace professional advice.