Paris law calculator: how many cycles before a crack grows to a dangerous size?

Enter the stress range, the crack lengths and the Paris constants to get the number of cycles for the crack to grow, the time and the stress intensity ranges.

Updated on
Your inputs
ksi

Value out of range

Value out of range

in

Value out of range

in

Value out of range

Value out of range

Value out of range

Value out of range

Results

Cycles to grow from a₀ to a_f

318,305

Time to grow, in days
159.2 days
Stress intensity range at the start
7.94 ksi√in
Stress intensity range at the end
28.07 ksi√in
Initial crack growth rate
0.180 µin/cycle

Fatigue cracks grow a tiny amount at each load cycle, and the time between a detectable crack and a failure can be long or short depending on the stress. The Paris law calculator takes the stress range, the geometry factor, the initial and final crack lengths, the constants C and m and the cycles per day, and gives the number of cycles to grow, the time in days, the stress intensity range at both ends and the initial growth rate.

How the calculation works

  • Enter the stress range Δσ, the geometry factor Y, the initial and final crack lengths, and the Paris constants C and m for the material.
  • Enter how many load cycles per day the part sees, to turn the cycles into time.
  • The stress intensity range is ΔK = Y × Δσ × √(π a), and the crack grows at the rate da/dN = C × ΔK^m.
  • The calculator integrates this law for a constant stress range: N = (a_f^(1−m/2) − a₀^(1−m/2)) / (C × (Y Δσ √π)^m × (1 − m/2)).

Example

A steel plate sees a stress range of 20 ksi with Y = 1.12. A crack of 0.04 in is found, and the plate fails when it reaches 0.50 in. With C = 3.6 × 10⁻¹⁰ and m = 3, the stress intensity range goes from 7.94 to 28.07 ksi√in. The initial growth rate is 0.18 µin/cycle, and the crack needs 318,305 cycles to grow, or about 159 days at 2,000 cycles a day.

Why it matters

Damage-tolerant design accepts that cracks exist and plans for how fast they grow. A Paris law calculation sets inspection intervals for aircraft, bridges, pressure vessels and cranes, shows how a small cut in the stress range lengthens the life a lot, and gives a feel for why a crack that seems stable can suddenly run.

Good to know

The calculator uses a constant stress range, a constant geometry factor and a single power law with fixed constants. It ignores the threshold, the effect of the stress ratio, retardation after overloads, crack closure, corrosion and the transition to fast fracture. Constants vary widely between materials and environments, so use values for your case. Treat the result as an order-of-magnitude estimate.

The Euler buckling calculator checks slender columns, the principal stress calculator finds main stresses, the Young’s modulus calculator covers stiffness, and the pressure vessel stress calculator finds wall stresses.

Frequently asked questions

What is Paris law?

Paris law says that the growth rate of a fatigue crack per load cycle, da/dN, is proportional to a power of the stress intensity range ΔK: da/dN = C ΔK^m. It describes the stable middle region of crack growth, between the threshold below which cracks do not grow and the final fracture. It is the base of damage-tolerant design.

What are typical values of C and m?

For ferritic-pearlitic steels in air, m is about 3, and C is about 3.6 × 10⁻¹⁰ in/cycle per (ksi√in)³, or 6.9 × 10⁻¹² m/cycle per (MPa√m)³. Aluminium alloys have m from 3 to 4 and a larger C. The constants depend strongly on the units, so always use C and m from the same source and in the same system.

What is the geometry factor Y?

It corrects the stress intensity for the shape of the crack and the part. Y = 1.12 is for a shallow edge crack in a wide plate, and Y = 1.0 for a central crack in an infinite plate. Cracks in finite plates, near holes or with a shape that changes as they grow have a Y that varies, and a constant value is only a first approximation.

How should I use the result?

As an inspection planning tool. Dividing the cycles by a factor of 2 to 4 gives a safe inspection interval, so that a crack is found before it reaches the final size. The final length should be below the critical crack size, which comes from the fracture toughness. Do not rely on it for life prediction without data for your material.