Long-term deflection creep multiplier calculator

Enter the immediate deflections, the compression steel, the span, the duration and the limit to get the multiplier, the added deflection and the ratio to the limit.

Updated on
Your inputs
in

Value out of range

in

Value out of range

%

Value out of range

ft

Value out of range

Results

Deflection after the partitions are in place

0.52 in

Long-term multiplier λ
1.60
Additional long-term deflection
0.32 in
Allowable deflection
0.60 in
Ratio to the allowable deflection
0.87
Within the limit

The long-term deflection calculator gives the creep multiplier λ of ACI 318, the additional long-term deflection, the deflection after the partitions are installed and its ratio to the allowable limit, from the immediate deflections, the compression steel, the span and the duration of the load.

How the calculation works

  • Enter the immediate deflections caused by the sustained load and by the live load.
  • Enter the compression reinforcement ratio, the span, the duration of the sustained load and the limit.
  • The calculator finds the multiplier λ, the additional long-term deflection, the deflection after the partitions and its ratio to the limit.

Example

A beam of 24 ft has an immediate deflection of 0.20 in. from the sustained load and 0.20 in. from the live load, with 0.5 percent of compression steel and a load that lasts 5 years or more. The multiplier is 2.0 / (1 + 50 × 0.005) = 1.60, so the additional deflection is 1.6 × 0.20 = 0.32 in. The part after the partitions is 0.32 + 0.20 = 0.52 in., against L/480 = 0.60 in., a ratio of 0.87.

Why it matters

The calculator helps structural engineers, designers and students to check the serviceability of concrete beams and slabs, to see how much the deflection grows with time, and to choose between more compression steel, a deeper section or a camber.

Good to know

Compute the immediate deflections with the effective moment of inertia of the cracked section, under the sustained load and the live load separately. Count in the sustained load the dead load and about a quarter of the live load for an office. If the ratio is over 1, a camber can offset the dead load deflection, and a deeper section is more efficient than extra steel.

The beam deflection calculator gives the immediate deflection of a beam, the beam camber calculator gives the camber for the dead load, the RC beam flexural capacity calculator gives the moment strength of a concrete beam and the one-way slab minimum thickness calculator gives the thickness without deflection checks.

Frequently asked questions

What is the long-term deflection multiplier?

A concrete member under a sustained load keeps deflecting with time because of creep and shrinkage. ACI 318 gives the additional long-term deflection as λΔ times the immediate deflection caused by the sustained load, with λΔ = ξ / (1 + 50 ρ'). The factor ξ is 1.0 at 3 months, 1.2 at 6 months, 1.4 at 12 months and 2.0 at 5 years or more, and ρ' is the ratio of the compression steel at the middle of the span.

Why does the compression steel help?

Compression steel carries part of the compression in the concrete and holds it from creeping. A beam with 1 percent of compression steel has a multiplier of 2.0 / 1.5 = 1.33, instead of 2.0 without compression steel. For a continuous beam, ρ' is taken at the middle of the span, and for a cantilever at the support. The effect is small for a lightly reinforced slab and it is greater for a deep beam.

Which part of the deflection is checked?

The code limits the part of the total deflection that occurs after the installation of the non-structural elements, which is the long-term deflection from the sustained loads plus the immediate deflection from the extra live load. The limit is L/480 for a member that supports elements likely to be damaged by large deflections, and L/240 for one that supports elements not likely to be damaged.

What does the calculator leave out?

The calculator uses the immediate deflections that you compute with the effective moment of inertia of the cracked section, which it does not find. It does not include the thermal effect, the differential shrinkage, the deflection of the supports or the camber. The sustained load must include the dead load and the part of the live load that stays for long. Follow the code of your country for the factors.

Was this calculator helpful?

Thanks for your feedback!

Results are estimates provided for information purposes. They do not replace professional advice.